Skip to content
Get matched

Guides / Design

Rib design for injection molded parts: thickness, height, draft and spacing

November 15, 2026

A rib is a thin wall that stands on a part surface to add stiffness without adding thick material. The usual rib rules are: thickness 50 to 60 percent of the nominal wall, height up to about 3 times the wall, draft of 0.5 to 1 degree per side, a base radius of roughly a quarter to half the wall and spacing of at least 2 to 3 times the wall between ribs. These are starting points for typical amorphous and semi-crystalline resins. The sections below explain the reason for each number and the trade-offs.

Why ribs exist

A flat plastic panel bends easily. Making it thicker works, but thick plastic is costly: it uses more resin, cools slowly and sinks and warps. A rib raises stiffness by adding depth to the cross-section. Bending stiffness grows with the cube of the section depth, so a modest rib adds a large gain at small material cost.

Ribs also help in other ways: they support bosses, guide flow across a part, stiffen edges and strengthen a joint. Used badly they create the defects they were meant to avoid.

Rib design rules at a glance

Typical values, with the wall thickness written as t. The exact numbers depend on the resin, the grade and the cosmetic need.

Feature Typical guideline
Rib thickness at the base 50 to 60 percent of t (40 to 50 percent if the opposite face is glossy or textured)
Rib height Up to about 3 t, taller only if tooling and fill allow
Draft per side 0.5 to 1 degree, more with texture
Base radius About 0.25 t to 0.5 t
Tip Small radius or flat, not sharp
Spacing between ribs (center to center) At least 2 to 3 t
Intersections Avoid thick junctions, stagger or use gussets

Worked example: nominal wall 2.5 mm. Rib thickness at the base 1.25 to 1.5 mm. Rib height up to about 7.5 mm. Spacing at least 5 to 7.5 mm. Draft 1 degree per side. Base radius 0.6 to 1.2 mm.

Rib thickness and sink marks

Where the rib meets the wall, the plastic section is thicker than elsewhere. That spot stays molten longer and shrinks more as it cools. The shrinkage pulls the surface above it inward and leaves a dimple, a sink mark, on the opposite face. The thicker the rib compared with the wall, the stronger the effect.

Keeping the rib to about half the wall thickness cuts this effect. In semi-crystalline resins such as PP, nylon and POM, which shrink more, stay near the low end. On a glossy face, which shows every dimple, use thinner ribs or hide the effect with texture. See sink marks in injection molding for causes and fixes.

The base radius also matters. A sharp corner at the base of a rib concentrates stress and can crack. A large radius creates a thick spot and a sink. The compromise of about a quarter to half of the wall thickness keeps both in check.

Rib height

Taller ribs give much more stiffness, but they are harder to fill and to eject. Common limits:

  • Up to about 3 t is a safe range for most designs.
  • Beyond that, the rib may not fill, may trap gas at the tip and may need a vent or be built as an insert in the mold.
  • Very tall, thin ribs are deep slots in the steel. They are cut by EDM, are fragile and can break or wear. They also cool poorly because it is difficult to place cooling near them.

If you need more stiffness than a 3 t rib gives, add a second rib, change the rib pattern or increase the wall thickness slightly. Do not solve it by thickening the rib.

Draft on ribs

Ribs need draft on both faces. Because the part shrinks onto the mold steel, a straight-sided rib grips the steel and drags during ejection. Result: scuffing, stuck ribs, stretched ribs or broken ejector marks.

Typical draft is 0.5 to 1 degree per side. Use more for tall ribs, textured faces and high-shrink resins. Add draft thickness into your thickness calculation: if the base is 1.4 mm and the draft is 1 degree on a 7.5 mm rib, the tip is about 1.1 mm. See draft angle in injection molding for more detail.

Spacing and layout

Ribs placed too close together make a narrow slot in the steel between them. That steel fin cools poorly, becomes hot and distorts. It is also difficult to polish. At least 2 to 3 times the wall thickness between neighboring ribs is a normal minimum.

Layout guidelines:

  • Run ribs in the direction of flow if possible. Ribs that run across the flow can create hesitation and weld lines.
  • Do not make grid patterns with thick intersections. Where two ribs cross, the section thickens. Use a staggered pattern or reduce the thickness at the junction, or connect with a small radius.
  • Support bosses with ribs, not solid mass. Use gussets or ribs from the boss to the wall. See boss design.
  • Keep ribs away from sharp edges so that the edge does not become a thick lip.
  • Place ribs on the non-cosmetic side. If both faces matter, think about a different stiffening approach, such as a curved panel or a flange.

Need a quote for a molded part? Get matched with a molding plant

Ribs, ejection and the mold

Because ribs are deep and narrow, the plastic grips the steel. Ejector pins or blades at the base of long ribs help to push the part off. Ejector marks may show on the surface of the rib. Where appearance matters, place ejectors on non-visible areas.

Deep ribs also affect venting. Air must leave the rib tip as melt arrives. If the tip is not vented, burn marks or short fills occur at the rib end. Many plants cut ribs as inserts so they can be vented or replaced. Raise this in the design review: the mold design review checklist lists the points.

Ribs and warpage

Ribs add stiffness, but they also change shrinkage. A panel with ribs on one side only will shrink more on the ribbed side and bend toward it. The effect is greater with thick ribs or in glass filled resin, where fibers align along the rib. Balance the pattern where you can, keep ribs thin and uniform, and consider a gentle crown on a large flat panel. See warpage in injection molding.

Checking stiffness

Before you add ribs, check whether you need them. A simple flat-plate calculation or a quick finite element study can estimate deflection. Bending stiffness of a rectangular section scales with the cube of its depth, so doubling the depth gives about 8 times the stiffness. Plastics creep, so calculate with a modulus at the temperature and time that applies, not the short-term datasheet value.

Then build samples and test them. A rib pattern that looks right on screen can sink, warp or be difficult to eject in real molding. Trial results are discussed in T1, T2 and T3 mold trials.

Design checklist

  1. Choose nominal wall t from the load, resin and flow length.
  2. Set rib base thickness to 50 to 60 percent of t (lower for glossy faces).
  3. Set rib height up to about 3 t.
  4. Add 0.5 to 1 degree of draft per side.
  5. Add a base radius of roughly 0.25 to 0.5 t.
  6. Space ribs at least 2 to 3 t apart.
  7. Check intersections for thick spots.
  8. Check ejector and vent locations with the plant.
  9. Check the opposite face for sink risk and decide if a texture can help.
  10. Confirm the plan in the DFM review. See DFM for injection molding.

Get a rib review before the mold is cut

Ask the plant to review your ribs in its DFM comments before it quotes the mold. A good answer lists which ribs it would thin, which it would shorten and where it would move ejectors. For other wall and thickness guidance, read wall thickness for injection molding.

We are a manufacturers’ representative for audited plastic injection molding plants. Buyers pay nothing: the plant pays us a commission on orders from buyers we introduce. Send an RFQ with your 3D model and we match it to the one partner plant whose lane fits, so you can get design feedback from a plant that runs parts like yours.

Frequently asked questions

Can I make a rib the same thickness as the wall?

You can, but it will usually leave a sink mark on the opposite face and create a thick spot that cools slowly. The common rule is a rib thickness of about half to 60 percent of the wall. For glossy or textured faces, stay at the lower end or add a deliberate surface feature.

How many ribs do I need?

Use the fewest that give the stiffness required. Stiffness increases quickly with rib height, so one taller rib often beats two short ones. Check the stiffness with a hand calculation or a simple simulation, and test a sample before you add more ribs.

Do ribs need draft?

Yes. Ribs are deep, narrow features that grip the steel as the part shrinks, so they need draft on both sides to eject cleanly. A typical draft is 0.5 to 1 degree per side, more with texture. Zero draft ribs cause drag marks, stuck parts and damaged steel.

Need a quote for a molded part?

Send the model. We match it to the partner plant whose lane fits and reply within 24 business hours. Free for buyers.

Get matched with a molding plant

Keep reading