Guides / Design
Boss design for injection molding: screws, inserts, ribs and sink control
November 20, 2026
A boss is a cylindrical feature that holds a screw, a threaded insert or a pin. A good boss has an outer diameter of about twice the screw size, a wall that is thinner than the part wall behind it, a generous fillet at the base, ribs that tie it to the surrounding wall and a hole depth that matches the screw length. These features keep the boss strong without causing sink marks, voids or cracks. The ranges below are typical rules of thumb. Confirm the numbers for your resin and screw with the plant and the fastener supplier.
Boss geometry at a glance
| Feature | Typical guideline | Why |
|---|---|---|
| Boss outer diameter | About 2 to 2.5 times the screw outer diameter (self-tapping) | Enough material around the thread to resist hoop stress |
| Boss wall thickness | About 50 to 60 percent of the nominal wall | Limits the thick section that causes sink marks |
| Base fillet radius | At least about 0.25 times the nominal wall, not sharper than about 0.5 mm | Reduces stress concentration at the root |
| Outside draft | About 0.5 to 1 degree | Easy ejection |
| Hole draft | About 0.25 to 0.5 degree, or none by agreement | Hole core stays accurate |
| Support ribs | 3 or 4 ribs, thickness about 50 to 60 percent of the wall | Strengthen the boss and tie it to the wall |
| Hole depth | Screw engagement plus clearance, hole deeper than the screw tip | Prevents bottoming and cracking |
| Thread engagement | At least about 2 times the screw outer diameter | Pull-out strength |
These are starting points. Resin stiffness, creep and the load on the joint change them.
Outer diameter and wall thickness
The boss has to resist the hoop stress made by a screw as it cuts or forms a thread. If the boss is too small, the wall cracks, perhaps hours after assembly. A boss outer diameter of about twice the screw outer diameter is a common starting point for self-tapping screws in many thermoplastics, and more for brittle resins.
Thickness has a second limit. A boss that is too thick makes a mass of plastic behind the outer surface. That mass cools last and shrinks, pulling the visible wall inward and leaving a sink mark. To limit this, the boss wall is kept to roughly half to 60 percent of the nominal wall where it meets the part. See sink marks in injection molding and injection molding wall thickness.
The two rules push in opposite directions. When they conflict, you can:
- Core out the boss to leave a hole deep enough for the screw, so the wall around it stays thin.
- Switch to a resin with higher strength, so a thinner wall can carry the screw.
- Use a heat-set insert, which spreads the load differently.
- Accept a light texture on the outside surface to hide a small sink.
The base: fillet and connection to the wall
A boss that stands alone on a flat wall is weak at the root. A sharp corner at the base concentrates stress, and a crack starts there. Add a fillet at the base. A radius of at least about a quarter of the nominal wall is a common minimum, and more is better, up to the point where the fillet itself makes a thick section.
Where the boss sits near a side wall, connect it to that wall with a rib, not by merging it into a thick block. A boss attached to the side wall by a full web of plastic creates a thick section that sinks. A boss joined by a thin rib gets support without the mass.
Ribs and gussets
Ribs tie the boss to the wall and stiffen it against side loads. Typical practice:
- Use three or four ribs around a freestanding boss, or one or two toward the nearest wall.
- Make the rib thickness about 50 to 60 percent of the nominal wall at its root, so the rib does not sink.
- Make the rib height up to about two thirds of the boss height, or less, with a small gap at the top so the rib does not weaken the boss rim.
- Add draft on the ribs, usually 0.5 to 1 degree per side.
Rib rules are covered in more detail in rib design in injection molding.
Hole depth and pilot size
The hole inside the boss should be deeper than the screw will reach, so the tip never touches the bottom and does not jack the boss out of the wall. Common practice is to leave a clearance of about one screw diameter or at least a few millimeters below the screw tip. A blind hole is formed by a core pin from the mold. Long core pins bend under injection pressure, so a deep, narrow hole is hard to hold. If the hole is deep and slender, ask the plant for a pin with support, or make a shorter boss.
The pilot hole diameter depends on the screw type and the resin. Screw suppliers publish a recommended pilot hole for thread-forming and thread-cutting screws in common resins. Use their figure and have the plant confirm it by trial. The hole is usually dimensioned at the top and tapered by draft, so state at what depth the diameter applies.
Need a quote for a molded part? Get matched with a molding plant
Heat-set and ultrasonic inserts
A metal threaded insert pressed or melted into a boss gives a stronger and more repeatable thread than a screw cut directly into plastic. It also survives repeated assembly and disassembly.
- The insert supplier gives the hole diameter, the hole depth and the boss outer diameter. The boss outer diameter is commonly about twice the insert outer diameter, and the supplier’s figure takes priority.
- Add a lead-in at the top of the hole, a small chamfer or counterbore, so the insert starts straight.
- Leave space under the insert for displaced plastic to flow, using a deeper hole or small relief.
- Specify the insertion method (heat, ultrasonic or press-in) and the pull-out and torque requirements.
- If the insert is molded in rather than installed after, see insert molding, and for the comparison with other joining methods see heat staking vs insert molding.
Resin matters
- Brittle or glass filled resins need larger bosses and more generous fillets, since stress concentrates and weld lines weaken the boss.
- Soft, creeping resins such as PE and some PP grades lose clamp load over time. An insert or a metal sleeve helps.
- Amorphous resins such as ABS and PC are sensitive to stress cracking from over-torque and from some chemicals. Specify a torque limit.
- Nylon absorbs moisture, which changes dimensions and strength. Allow for it in hole size and joint design.
Check the resin supplier’s design guide for the recommended screw type and boss size. For a comparison of resin properties see ABS vs PC/ABS.
Avoiding weld lines and voids
When the melt flows around a core pin, it splits and rejoins on the far side, making a weld line through the boss wall. This is a weak plane exactly where the screw creates stress. Ask the plant where the weld lines will fall, using a flow study if the part is critical. See weld lines in injection molding. Moving the gate or changing the boss position can shift the line away from the boss.
A thick boss base can also trap a void inside. Hold pressure and a gate close to the thick section help the plant pack it out.
Checklist for the drawing and the design review
- Screw size, type and the torque value stated on the drawing.
- Boss outer diameter, hole diameter and depth with the draft stated.
- Boss wall as a share of the nominal wall, checked against sink risk.
- Fillet radius at the base.
- Ribs: number, thickness, height and draft.
- Insert type, supplier and installation method if used.
- Gate and weld line position near each boss, reviewed with the plant.
- Sample tests: screw torque-out and pull-out on T1 parts.
Working with a rep
We are a manufacturers’ representative for injection molding plants. Buyers pay nothing for the introduction; the plant pays us a commission on orders from buyers we introduce. If your part has screw bosses or inserts, mark them in the RFQ and we route it to the partner plant whose lane fits the part. Send an RFQ with your STEP model and the screw or insert data sheet.
Frequently asked questions
How thick should the wall of a screw boss be?
As a typical guide, the boss wall is about 50 to 60 percent of the nominal wall of the part, so the thick section behind the boss does not cause a sink mark on the outside. The boss outer diameter is commonly about twice the screw outer diameter for self-tapping screws. Confirm the figures with your screw and insert supplier and with the plant, since resin and load change them.
Should I use a self-tapping screw or a heat-set insert?
Self-tapping screws cost nothing extra in assembly parts, but the thread in plastic can strip when the part is serviced repeatedly. Heat-set or ultrasonic inserts give metal threads that survive many assembly cycles and carry higher loads. Choose inserts when the joint is opened often or carries a high pull-out load.
Why do bosses crack?
Common causes are a boss outer diameter that is too small for the screw, a pilot hole that is too small, over-torque, sharp corners at the base, a resin that creeps or is brittle (for example some glass filled grades) and a weld line through the boss. Fix the design first, then check assembly torque.
Need a quote for a molded part?
Send the model. We match it to the partner plant whose lane fits and reply within 24 business hours. Free for buyers.