Guides / Design
Ejector pin marks: where they land, how to place them and how to hide them
November 21, 2026
An ejector pin mark is the small round impression left on a molded part where a steel pin pushed it out of the mold. Every part ejected by pins has them. You cannot get rid of them, but you can decide where they land, how deep or high they are and whether they are visible. The way to do that is to agree on pin locations and mark limits with the plant before the mold design is approved, not after the first samples show circles on the visible face.
This post covers why marks occur, where pins should go, how to control height, how to hide the marks and what to put in the drawing.
Why ejector pin marks exist
When the mold opens, the part stays on one half, usually the core or “B” side. A plate with steel pins then pushes forward and forces the part off the core. The pin tips touch the part, and the contact area shows as a mark.
The mark is a small difference in surface texture, gloss or height. Typical causes:
- The pin tip sits slightly above or below the surrounding cavity surface, which leaves a shallow recess or a small raised disc.
- The pin tip has a different finish from the surrounding steel, so the gloss differs.
- The pin pressed on soft plastic and left a dent or stress mark.
- A small amount of flash or a thin film formed around the pin gap.
A pin set slightly below the surface leaves a raised disc. A pin set slightly above it leaves a shallow circular recess. Which one you can accept depends on the function of the face. A raised disc can stop a part sitting flat. A recess can trap dirt or look odd in a gloss face.
Which side gets the marks
The side with the pins is the ejector side. The plant designs the mold so that the part stays on that side when it opens. Draft, texture and undercuts all push the part toward one half or the other.
Tell the plant which face is the cosmetic or “A” face and which is the hidden one. The plant can then keep the cosmetic face on the cavity side, with no pins, and put the marks on the inside, on the “B” face. This single decision removes most visible marks. See parts of an injection mold for how the two halves are laid out.
Where to place pins
The pin must push on a strong area of the part. If it pushes on a thin, unsupported wall, it can punch through or distort it.
Good places for pins:
- At the bottom of ribs. The rib is a stiff, thick area, and a pin there pushes the part with little deflection.
- Under bosses and on boss walls. Often a sleeve ejector, which is a ring around a core pin, is used here.
- Along the part perimeter or on flanges, where the wall is stiff.
- Close to the areas that grip the core most, such as deep cores and tall walls, where the part sticks hardest.
- Spread evenly so the part comes off straight and does not tilt or twist.
Poor places for pins:
- On a cosmetic face.
- On a thin wall far from any support.
- On a sealing or mating face.
- In an area that will be textured, unless the plant plans for it.
- On a surface where the pin would catch an undercut.
Pin size and count
Pins used in injection molds commonly range from about 2 mm to 12 mm in diameter. A small pin concentrates force and can mark or punch the part. A larger pin spreads the force. A few larger pins are usually better than many tiny ones, if the geometry allows. Tiny pins also bend and break more often.
The plant calculates the number and size from the ejection force, which depends on the part area on the core, the draft, the surface finish and the resin shrinkage. More draft means less force. See draft angle in injection molding.
Controlling mark height
Specify the limit. If the drawing is silent, the plant decides.
| Face | Suggested approach |
|---|---|
| Hidden internal face | Allow marks; state a maximum height or depth |
| Visible but non-critical face | Allow marks only in marked zones; tighter limit |
| Cosmetic face | No marks allowed; ejection must be through other faces |
| Mating or sealing face | No marks, or marks only below the surface in a pocket |
Typical limits are a fraction of a millimeter. Pick a number your assembly can tolerate, write it on the drawing and ask the plant whether it can hold it. Tight limits need good pin fit and regular checks as the mold wears.
Need a quote for a molded part? Get matched with a molding plant
Ways to hide ejector pin marks
If you cannot avoid marks on a visible area, choose one of these methods.
Move them
Redesign so pins act on a rib, a boss or the inside of the part. This is the cheapest and most reliable fix.
Add ejector pads
Add a small raised pad on the inside face and let the pin push on the pad. The mark sits on the pad, which is not a functional surface. Keep pads small, with a thickness close to the wall so they do not cause sink on the outside.
Use a pocket
The mark is placed in a small recess so that the mark sits below the level of the surrounding surface. A part can then sit flat even if the pin leaves a raised disc.
Add texture
Texture on the ejector face camouflages marks. A coarse texture hides them well. Note that the pin tip is smooth, so on a textured face the pin spot can look glossy unless the plant textures or matches the pin tip. See injection mold texture.
Use another ejection method
- Stripper plate: a plate that pushes the whole rim of the part. Good for round, thin-walled parts such as caps and cups. It leaves no pin marks, only a ring at the rim.
- Sleeve ejector: a ring around a boss or core pin. Used for round features.
- Blade ejector: a thin rectangular pin for ribs.
- Air ejection: compressed air through a valve helps release thin or deep parts.
These cost more than pins and need space. Ask the plant which fits your geometry.
Other things that make marks worse
- Ejecting too early, when the part is still soft. A longer cooling time or better cooling lets the part set before the pin pushes.
- Too much pack, which makes the part grip the core harder.
- Too little draft or a rough core finish. Both raise ejection force.
- Worn or sticking pins, which can flash or lag. Maintenance matters. See injection mold preventive maintenance.
- Undercuts that force the part to be pulled hard. See undercuts in injection molding.
What to put on the drawing
- Mark the cosmetic faces and the faces where pin marks are not allowed.
- Mark the zones where ejector pins are allowed.
- State the maximum mark height or depth and the allowed direction, flush, raised or recessed.
- State the gloss or texture of the face, so the plant can match the pin tips if needed.
- Name the parting line and gate zones that must also stay clear. See parting line in injection molding.
Agreeing it with the plant
Add ejector layout to the mold design review. Ask the plant to show the pin positions on the 3D mold layout, with pin diameters and a note on any sleeves or stripper plates. The mold design review checklist lists the points to confirm before steel is cut. Agree a limit sample for the mark too, since “no visible mark” means different things to different people. See how to limit sample cosmetic defects.
Once the layout is agreed, send your RFQ with the cosmetic faces and mark limits stated up front. We are a manufacturers’ representative. We route your package to the partner plant whose lane fits the part, it is free for buyers. The plant pays us a commission on orders from buyers we introduce, and you order directly from the plant.
Frequently asked questions
Can ejector pin marks be removed completely?
Not with pins. Any part pushed out by pins carries a mark. You can move the marks to a hidden face, hide them with texture or a pocket or eject without pins by using a stripper plate, sleeves or air. The best fix is to decide where marks may go before the mold design is approved.
How deep or high can an ejector pin mark be?
It depends on the part. A common approach is to limit the mark to a very small height or depth, often a fraction of a millimeter, and to state the limit on the drawing or in the PO. Mating faces and sealing faces need a tighter limit than hidden faces.
Why do ejector pins sometimes cause white stress marks?
If the part is still soft or the pin force is concentrated on a small area, the plastic can be stressed or deformed at the pin. This shows as a white or glossy spot, mostly on ABS, PC and similar resins. More pin area, better cooling and a smoother ejection reduce it.
Need a quote for a molded part?