The parting line in injection molding is the line on the part where the two mold halves meet, and it is placed where the part can release from the mold in the opening direction. It leaves a thin witness mark, and it is a common site for flash. Where you put it decides cosmetic quality, how many draft and undercut problems you have and how complex, and costly, the mold becomes. Mark your cosmetic zones on the drawing and approve the location at design review. This page explains the options and the trade-offs.
What the parting line is
A mold has two main halves: the cavity side, which usually forms the outside or visible face, and the core side, which usually forms the inside and carries the ejector system. The parting line is the surface where the halves touch. When the mold closes, the plastic is injected, and when the mold opens, the part must come away from one half and be pushed off the other.
Because the two halves meet at a joint, a thin line remains on the part. A well-fitted mold gives a small witness line. A worn or poorly fitted mold gives flash, a thin film of plastic escaping through the joint. See flash in injection molding for causes and fixes.
What decides the location
Four things drive where the parting line goes:
- Release direction. The line sits at the widest point of the part in the mold opening direction, so no part of the shape traps itself. Features that cannot release need slides or lifters. See undercuts in injection molding.
- Draft. Draft angle is measured from the pull direction, so the parting line is the pivot from which the draft runs both ways. See draft angle in injection molding.
- Cosmetics. The line should be where it is least visible or least objectionable.
- Mold cost. A flat parting line is cheapest. A stepped or curved one costs more to machine, fit and maintain.
Placement options and trade-offs
| Option | Effect on appearance | Effect on cost and risk |
|---|---|---|
| Flat line at the outer edge of the part | Hidden on a sharp edge or lip. Good for most housings. | Lowest cost, easiest to maintain. |
| Line on a visible flat face | Shows as a line across the face. Poor for cosmetic parts. | Same cost as flat, but may be rejected at inspection. |
| Line in a groove or a step | Hidden by the shadow of the step. | Slightly higher cost, as it needs a feature added. |
| Line on a curved surface | A stepped or curved parting surface follows the shape. Line can be hidden on the curvature. | Higher machining and fitting cost, harder to keep tight. |
| Line along a round part’s side | Shows as a line along the length, if the mold splits sideways. | Needs slides, or two halves of a split cavity. |
| Line at the end of a round part | No line on the barrel; the line is at the end face. | Needs draft along the length and a core that pulls axially. |
For a round part such as a cap or a cup, the choice of line direction is one of the main design decisions. A sideways split leaves a line along the full length. An axial pull leaves no line along the length but needs draft on the full side wall.
Cosmetic tactics
- Put the line on a sharp outer edge. The edge hides the line because light does not run across it. The sharp edge also helps the steel, since a sharp shut-off is stronger than a thin feather of steel.
- Avoid a radius across the parting line. A rounded edge over the parting line forces a thin sliver of steel at the joint that wears or breaks and leaves a visible line or flash. A small flat or a tiny step at the edge is more durable.
- Use texture. A texture hides the line better than a polish, but the line and texture should be discussed with the mold maker, because texture must flow cleanly across the joint. See injection mold texture.
- Use a step or shadow line. A design with a small step at the parting line, like a panel gap, makes the line look intentional.
- Keep gates and ejector marks away from the line, so witness marks do not add to each other. See ejector pin marks.
- Think about assembly. If two molded parts meet, line up their parting lines with the visible seam between them.
Need a quote for a molded part? Get matched with a molding plant
Flash risk at the parting line
Flash tends to occur where the line is long, curved or thin. The fit of the mold halves, the clamp force, the injection pressure and the resin viscosity all matter. Low viscosity resins, such as nylon and some PP, flash more easily than stiff resins.
Design helps:
- Avoid very thin edge features right at the parting line.
- Keep shut-off surfaces wide enough to resist wear, and with enough angle to close cleanly. A shut-off of about 3 degrees or more is a common guideline for tight, sliding-free closure, and the mold maker sets the final value.
- Keep the line short and simple when possible.
- Specify an allowable flash height, such as “flash maximum 0.1 mm”, where the function needs it.
Mold maintenance matters as much as design. A parting line that was tight at T1 can open as the mold wears. See injection mold preventive maintenance.
Parting line and the mold side that keeps the part
The location of the line also decides which half holds the part when the mold opens. Usually the part stays on the core side, where the ejectors push it off. If the cosmetic face is on the core side, the ejector pins sit behind the visible face, which is less than ideal. If the cosmetic face is on the cavity side, the part may cling to the cavity and need a mold design to ensure it stays on the core.
Discuss this at design review: where are the visible faces, which half forms them, and where will the ejector pins mark the part? See mold design review checklist and parts of an injection mold.
What to mark on your drawing
A drawing helps the plant when it states:
- Cosmetic zones, marked with a letter or color, such as Zone A (no marks), Zone B (minor marks allowed) and Zone C (hidden).
- A preferred parting line location, or a note that it must not cross Zone A.
- The maximum witness line and flash, for example “parting line witness 0.1 mm maximum, no flash on Zone A”.
- Texture or polish per face.
- Gate and ejector zones that are allowed.
- The mold opening direction, if you have a view about it.
If you only want the plant to propose, say so in the RFQ, and ask for the proposed line to be shown in the design review package.
Checks on samples
At T1 and later, ask the plant to report:
- Photos of the parting line along its length, with a scale.
- Measurement of the witness line step or mismatch, where the function needs it. A mismatch between halves of 0.05 to 0.1 mm is a common range in practice, but the right value depends on the part and the mold.
- Flash check, especially after the mold has run for a few thousand shots.
- A note on the repair method if the line is poor, such as re-fitting the shut-off.
Include the criteria in the sample approval. See first article inspection for plastic parts.
Send the part with cosmetic zones marked
plasticmoldingfactories.com is a manufacturers’ representative for audited plastic injection molding plants. Buyers pay nothing; the plant pays us a commission on orders from buyers we introduce. Send the drawing with your cosmetic zones in an RFQ, and we route it to the one partner plant whose lane fits, and you agree the parting line with that plant directly.
For a neutral overview of the process and its terms, the injection moulding article on Wikipedia is a useful reference.
Frequently asked questions
Can a molded part have no visible parting line?
Not in practice. Every molded part has a parting line where the mold halves meet. You can make it faint, hide it at a sharp edge or step, or place it on a non-visible face. A well-made and maintained mold leaves a very thin witness line, but it is rarely invisible.
Who decides where the parting line goes?
The mold designer proposes it, based on draft, undercuts and part function. The buyer should mark cosmetic zones and approve the location at design review. If you do not mark it, the plant will choose the cheapest option, which may not be where you want it.
Why does the parting line flash after the mold has run for a while?
Wear, damage, debris on the shut-off, insufficient clamp force or too much pressure can all open the parting line. Ask the plant for the cause and a maintenance record. Repeated flash on the same spot often points to a worn or damaged shut-off that needs repair.