Undercuts in injection molding: slides, lifters and design workarounds
November 10, 2026
An undercut is any feature that stops a molded part from pulling straight out of the mold in the direction the mold opens. Side holes, clips, snap hooks, external threads, grooves and internal ribs under a lip are typical examples. You release an undercut with a slide, a lifter, a collapsible core or an unscrewing mechanism, or you redesign the part so that the undercut disappears. Each mechanism adds cost, so the cheapest undercut is the one the design removes.
Why undercuts matter for cost
A mold with two plates opening along one axis is the simplest and cheapest design. Every undercut adds a mechanism that moves in another direction. That mechanism needs design time, machined steel, fitting, a way to move and lock, and maintenance for the life of the mold. See injection mold tooling cost for how this stacks with cavities, steel and finish.
Typical effects of one slide:
- A higher mold cost (a typical range is one thousand to several thousand US dollars per simple slide, more for large or hydraulic ones).
- A bigger mold base, because slides need space around the cavity.
- A wear point where flash or a witness line can appear.
- Longer mold maintenance and more spare parts.
- Sometimes a longer cycle if the slide stroke is long.
Four ways to release an undercut
Side action (slide)
A slide is a block of steel that forms the undercut feature and moves sideways, at right angles to the mold opening, before the part is ejected. An angled pin, called an angle pin or finger cam, mounted in the other mold half drives the slide as the mold opens. Angle pins commonly sit between about 10 and 25 degrees (typical). Hydraulic or pneumatic cylinders drive the slide when the stroke is long or when the slide must move before the mold opens. A locking heel holds the slide shut against injection pressure.
Use a slide for: side holes, external threads, side clips and grooves on the outside of the part.
Lifter
A lifter is an angled rod or blade that forms an undercut on the inside of the part, usually a hook or a rib under a lip. During ejection, the lifter rises with the ejector plate and also moves sideways along an angle, so it clears the undercut as the part moves up. Lifters are cheaper than slides because they ride on the ejector system, but they need space, strength and a stroke long enough to clear the undercut with margin.
Use a lifter for: internal snap hooks, internal ribs under a lip and small internal side features.
Collapsible core
A collapsible core is a segmented core that folds inward after molding to clear an internal undercut, such as an internal thread or a wide internal groove around the whole circumference. It is complex, expensive and has a limited life. Plants use it for closures, caps and fittings with high volumes.
Use a collapsible core for: internal circular undercuts where a slide or lifter cannot reach.
Unscrewing mechanism
For molded threads, the core or cavity rotates out of the thread after molding, driven by a hydraulic motor or a rack and pinion. It adds cost and cycle time, yet it gives clean, accurate threads without a witness line. Some external threads avoid it altogether, as shown in the workarounds below.
Use unscrewing for: full molded threads on caps, bottles, couplings and fittings.
Bump-off undercuts
In flexible resins, a shallow undercut can be forced off the core without any moving mold part. The part flexes as it leaves the mold. The conditions:
- The resin is soft: TPE, TPU, PE or soft PP.
- The undercut is shallow and rounded, with generous radii.
- The part has room to deform and recover.
- The undercut is on a feature that is not under heavy load in service.
Do not use a bump-off in rigid or glass filled resins such as PC, PA with glass fiber or PBT. The part cracks or whitens at the undercut. Ask the plant to check strain at the undercut, not only the geometry.
Design workarounds that remove the undercut
The most useful work happens in the design review before the mold exists. These changes save the most.
- Move the undercut to the parting line. A feature that sits on the line where the two mold halves meet can be formed without a slide. This often changes where the parting line goes. See parting line in injection molding.
- Use a pass-through opening (shut-off). A side window can often be formed by letting the core and cavity touch through the wall. Steel meets steel at a shut-off face. The angle of the shut-off, commonly at least 3 degrees and often 5 degrees or more (typical), keeps wear low. The opening gets a draft, and the side wall of the window cannot be perfectly square.
- Replace a snap hook with a window beneath it. A hook that points outward needs a slide. If you cut a window in the wall below the hook, the core forms the hook underside through the window, and no slide is needed. This is the single most common workaround. See snap-fit design.
- Change the direction of the feature. A clip that points along the mold opening needs no mechanism.
- Split the part into two parts. A housing with side features can become a cover and a base, each molded in the opening direction. This adds an assembly step and a joint.
- Do the feature as a secondary operation. A small side hole can be drilled after molding, if the volume is low and the position tolerance allows. At high volume this is rarely cheaper than a slide.
- Let the thread end at the parting line. An external thread that runs across the split can be molded without unscrewing, at the price of two small flats where the mold halves meet. Check that the mating part tolerates the flats.
Need a quote for a molded part? Get matched with a molding plant
Design rules when an undercut is unavoidable
- Keep it small. A shallow undercut needs a shorter slide stroke and a smaller slide.
- Give the slide room. Leave a flat, uninterrupted area on the part for the slide, with draft on the sliding faces.
- Add draft on the slide direction. The feature still needs draft along its own pull direction. See draft angle in injection molding.
- Group undercuts on the same side. One slide can form several features if they are in line.
- Avoid undercuts on cosmetic faces. A slide leaves a witness line where it meets the cavity.
- Allow for wear. Ask for hardened steel on the sliding surfaces and a lubrication point in the mold design.
Undercuts and tolerances
A moving mold part adds tolerance. Where a slide closes against the cavity, the two steel faces meet with a small clearance, and the position of the feature depends on how well the slide returns to the same place on every shot. Features formed by a slide can therefore hold a slightly wider tolerance than features formed by the fixed core and cavity (typical). If a hole or a hook position is critical to function, tell the plant at the design review so it can choose a locking method and a datum that keep that feature accurate. See injection molding tolerances for typical ranges.
Slides also leave a visible line. On a textured or polished face, the line can show as a change in gloss. If the face is visible in the final product, ask the plant to place the slide split on an edge or a radius, or to hide it behind an assembly feature.
What to put in the RFQ and the design review
- Mark every undercut on the drawing or in a short list.
- Ask the plant which undercuts need a slide, a lifter or another mechanism, and the cost of each.
- Ask which design changes would remove them, with a sketch.
- Agree which cosmetic faces must stay free of witness lines.
- Ask about slide material, hardness and the maintenance plan.
Compare quotes on the same list, since a quote that leaves out a slide is not a lower price, only an incomplete one. For the full list of checks before tooling, see mold design review checklist.
Working with a rep
We are a manufacturers’ representative for injection molding plants. Buyers pay nothing for the introduction; the plant pays us a commission on orders from buyers we introduce. If your part has side features, list them in the RFQ and we route it to the partner plant whose lane fits the part and the press range. Send an RFQ with your STEP model and a mark-up of the undercuts.
Frequently asked questions
Can an undercut be molded without a slide?
Sometimes. A shallow undercut in a flexible resin such as TPE, PE or soft PP can be forced off the core (a bump-off), if the feature is rounded and the strain stays low. Many undercuts can also be moved into the parting line or replaced by a pass-through opening formed by the core and cavity touching. Rigid resins and sharp edges usually need a slide or lifter.
How much does a slide add to the mold price?
As a typical range, a simple slide on a small to mid-size mold adds from about one thousand to several thousand US dollars, and a large, hydraulic or double slide adds more. Region, mold size and steel decide the final number. Ask the plant to price each slide separately in the quote so you can see what a design change saves.
Do undercuts affect cycle time and part quality?
They can. A slide must move out before ejection and back before closing, which adds a small amount of time on some molds, and each slide is a wear point where flash can appear. Parting lines and witness marks also appear where a slide meets the cavity, which matters on cosmetic faces.
Need a quote for a molded part?
Send the model. We match it to the partner plant whose lane fits and reply within 24 business hours. Free for buyers.
Get matched with a molding plant