Injection molding tolerances: what is realistic by resin, dimension and feature

October 30, 2026

Realistic injection molding tolerances depend on the resin, the size of the dimension, the wall design and how well the process is controlled. As a rough guide for small parts, plus or minus 0.05 to 0.1 mm on a 25 mm dimension is achievable in stable amorphous resins such as ABS and PC. Semi-crystalline resins such as PP, HDPE and POM need about twice that. Tolerances tighter than this are possible, but they raise mold cost, cycle time and inspection effort, so reserve them for the features that need them.

Why molded parts vary

Every molded dimension is the mold dimension minus shrinkage. Shrinkage is the amount the plastic contracts as it cools from melt to room temperature. It depends on the resin, the wall thickness, the packing pressure, the mold and melt temperature and the flow direction. Anything that changes shrinkage from shot to shot changes the part size.

Four groups of causes:

  1. Resin: shrinkage rate, filler content, moisture uptake, lot-to-lot variation.
  2. Part design: thick walls shrink more than thin ones, ribs and bosses create local variation, flow direction orients fibers and molecules.
  3. Mold: build accuracy, wear, cavity-to-cavity differences, steel temperature, venting.
  4. Process: hold pressure and time, temperature, cooling time, the plant’s process control.

A tolerance is the range the plant can hold with all of these under control. The tighter it is, the less room remains for any of them to move.

Typical shrinkage by resin

Shrinkage ranges below are typical for unfilled grades. Datasheets for the specific grade give the figures to use, and glass fiber lowers them and adds a flow-direction difference.

Resin Typical shrinkage Notes
ABS 0.4 to 0.7 percent Stable, a good choice for tight fits
PC 0.5 to 0.7 percent Stable, sensitive to moisture and stress
PS and PMMA 0.2 to 0.7 percent Stable, brittle
PA6 and PA66 0.7 to 1.5 percent Absorbs moisture and grows with it
PA glass-filled 0.2 to 0.8 percent Differs along and across the flow
POM (acetal) 1.8 to 2.5 percent Crystalline, stable once conditioned
PBT 1.2 to 2.0 percent Lower with glass fiber
PP 1.0 to 2.5 percent High and variable, warps easily
HDPE 1.5 to 3.0 percent Highest of the common resins
TPE and TPU 0.5 to 2.5 percent Soft materials flex when measured

Low shrinkage does not alone mean tight tolerance. What matters more is how consistent the shrinkage is from shot to shot, and amorphous resins tend to be more consistent than semi-crystalline ones.

Typical achievable tolerances

The table gives plausible commercial and fine tolerance levels for a dimension of about 25 mm in a part with uniform walls, made by a plant with good process control. They are typical, not guarantees.

Resin group Commercial level Fine level
ABS, PC, PS, PMMA plus or minus 0.1 mm plus or minus 0.05 mm
PA glass-filled, PBT glass-filled plus or minus 0.1 mm plus or minus 0.05 mm
POM plus or minus 0.1 mm plus or minus 0.05 mm
Unfilled PA6, PA66 plus or minus 0.15 mm plus or minus 0.08 mm, after conditioning
PP plus or minus 0.2 mm plus or minus 0.1 mm
HDPE plus or minus 0.25 mm plus or minus 0.15 mm
TPE and TPU plus or minus 0.3 mm depends on hardness and shape

Two rules apply to all of them. Tolerance grows with the size of the dimension, because shrinkage works on the whole length. And tolerance across the flow direction differs from tolerance along it, particularly in filled resins.

The general tolerance standard for molded plastic parts is ISO 20457, which sets tolerance classes by material group and dimension size. A drawing can reference a class and mark the critical features separately. Check the current text at iso.org if you plan to cite it.

Which features hold tolerance and which do not

Some dimensions are controlled by the mold and others by the process. Plants know the difference, and your drawing should too.

  • Mold-controlled: dimensions formed within a single mold half, such as hole diameters formed by a core pin, or feature sizes inside one cavity. These hold tighter.
  • Process-controlled: dimensions across the parting line, over moving slides or across large spans. The parting line closing, slide positions and shrinkage all add variation, so tolerances here must be wider.
  • Warp-sensitive: flatness, straightness and roundness of large, thin or asymmetric parts. These depend on cooling and packing, not only on the mold.
  • Flexible features: snap hooks, thin walls and living hinges, which move when measured.

Hole diameters and distances between features on the same mold half are the easiest to hold. Overall length, width over a parting line and flatness on large panels are the hardest.

Design choices that make tolerance easier

  • Uniform wall thickness. It gives even shrinkage and less warp. See injection molding wall thickness.
  • Ribs rather than thick walls for stiffness, at the right thickness ratio.
  • Gates placed for even fill, and not in the middle of a critical feature.
  • Adequate draft, and a note on where the dimension is measured. See draft angle in injection molding.
  • Round features instead of long slots, and short spans instead of long ones.
  • Steel-safe design for critical features. The mold maker leaves extra steel on critical dimensions (cavities cut slightly small, core pins slightly large) and removes steel after T1 to reach nominal. It is cheaper to remove steel than add it. See steel-safe injection mold.

Need a quote for a molded part? Get matched with a molding plant

How to write a tolerance a plant can hold

  1. Mark critical-to-quality features. Everything else falls under a general tolerance class.
  2. Tie the tolerance to function. If a feature only needs a 0.3 mm clearance, say so, and do not tighten it by habit.
  3. Use geometric dimensioning where it helps. Position, flatness and profile tolerances describe fit better than plus and minus. See GD&T for molded parts.
  4. State the datum scheme. Choose datums the part can actually be held on during inspection.
  5. State the measurement conditions. Temperature, conditioning time and method.
  6. State sample size and capability for critical features, for example Cpk targets. See Cpk in injection molding.

Tight tolerances without a stated reason cost money and slow quotes. A plant that sees a drawing where every dimension is plus or minus 0.02 mm will either decline, or quote high.

Conditioning and measurement

Molded parts keep changing after ejection.

  • Post-mold shrinkage: semi-crystalline resins continue to crystallize and shrink for hours or days.
  • Moisture uptake: nylon grows as it absorbs water. A dry part and a conditioned part can differ by tenths of a millimeter on longer dimensions.
  • Temperature: plastics expand a lot more than metal. A part measured warm reads bigger than the same part at 23 degrees Celsius.
  • Stress relaxation: parts with molded-in stress move over time.

Agree a measurement protocol: parts at room temperature, conditioned for a set time, measured by a defined method such as CMM or optical, with a gauge or fixture for flexible parts. The same part measured by two different methods can disagree for reasons that have nothing to do with quality.

When tolerance needs help from other steps

If one feature needs a tolerance the molding process cannot hold, consider:

  • A post-mold operation such as reaming a bore or machining a face.
  • An insert, such as a metal bushing, to hold the critical feature.
  • A change of resin to a more stable one, such as glass-filled grade, if the function allows.
  • A fixture to hold the part while it cools, for flatness.
  • A design change to reduce the spans that need to be held.

Each of these adds cost, but it may be lower than the cost of a rising reject rate.

What to ask the plant

  • What tolerance class do you quote to, and for which resin?
  • Which of my critical features do you expect to hold, and which at risk?
  • What is the cavity-to-cavity variation on a multi-cavity mold?
  • What is the process capability for similar features?
  • What post-mold or conditioning steps are assumed?

Put the critical features in your request along with the other items in injection molding RFQ: what to send for a firm quote. For the checks on a plant’s measurement system, see how to choose an injection molding factory.

Next step

If you have a part with tolerances to review, send an RFQ with the drawing and mark the critical features. We are a manufacturers’ representative for audited plastic injection molding plants. We match the request to the one partner plant whose lane fits, you order from that plant directly, and it costs the buyer nothing. The plant pays us a commission on orders from buyers we introduce.

Frequently asked questions

What is a standard tolerance for injection molded parts?

For many small parts in stable resins, plus or minus 0.1 mm on a 25 mm dimension is a common commercial level, and plus or minus 0.05 mm is a fine level that needs more control. Larger dimensions, flexible resins and semi-crystalline resins need wider tolerances. Plants usually quote against a general tolerance standard plus any marked critical features.

Why do molded parts change size after molding?

Plastic keeps shrinking for hours or days after ejection as it finishes cooling and crystallizing, and some resins such as nylon take up moisture and grow. Annealing and conditioning stabilize the dimensions. Measure parts after a set conditioning time, for example 24 hours at room temperature, so results are repeatable.

Can tight tolerances be fixed by machining after molding?

Yes. Reaming, grinding or machining a feature after molding is a normal solution for one critical bore or face, but it adds cost and a process step. It is often cheaper than forcing the molding process to hold a very tight tolerance on every part. Discuss it with the plant at quote stage.

Need a quote for a molded part?

Send the model. We match it to the partner plant whose lane fits and reply within 24 business hours. Free for buyers.