Skip to content
Get matched

Guides / Materials

POM acetal injection molding: grades, design and process for gears and bearings

November 16, 2026

POM acetal injection molding makes stiff, low-friction parts such as gears, bearings, bushings, clips and pump components from polyoxymethylene, a semi-crystalline engineering plastic. It molds well at moderate temperatures but has high shrinkage, needs even wall thickness and has processing limits, including a clear ban on mixing with PVC. This guide covers grades, design rules, process points and what to put in the RFQ so the plant quotes the right material.

Why POM is used for gears and bearings

POM has a mix of properties that suit mechanical parts:

  • High stiffness and strength for an unreinforced plastic.
  • Low coefficient of friction and good wear resistance.
  • Good creep and fatigue resistance.
  • Low moisture absorption, so dimensions stay stable in humid conditions.
  • Good resistance to fuels, solvents and many oils.

The limits are equally clear. POM burns slowly, is attacked by strong acids and strong oxidizers, degrades under UV unless stabilized, and is notch sensitive. Sharp corners in a POM part reduce its toughness.

For a general background on the polymer, the polyoxymethylene article on Wikipedia is a neutral reference.

Homopolymer or copolymer

POM comes in two main families.

Property Homopolymer Copolymer
Stiffness and hardness Higher Slightly lower
Crystallinity Higher Lower
Melting point About 175 degrees C About 165 degrees C
Chemical resistance, hot water, alkalis Lower Better
Thermal stability in processing Narrower window Wider window
Centerline porosity in thick sections More likely Less likely

The values above are typical. Check the datasheet for the exact grade. In practice, homopolymer is chosen when stiffness, fatigue life and surface hardness come first. Copolymer is chosen when the part sees hot water, chemicals, alkaline cleaners or a long processing time, and when thick sections must be sound.

Grades to know

Base grades differ in melt flow, so choose by wall thickness and flow length. Besides the base grades, plants and resin suppliers offer:

  • Lubricated or low-wear grades, with PTFE, silicone or other additives, for bearings and sliding parts.
  • Glass filled or reinforced grades, for higher stiffness, with more anisotropy and wear on mating parts.
  • Impact modified grades, for tougher parts, at some cost in stiffness.
  • UV stabilized grades, for outdoor or light-exposed use.
  • Colored grades, where pigment can change shrinkage slightly.

State the full grade name in the RFQ. “Acetal” alone is not enough to quote or to match later.

Shrinkage and dimensional control

POM has high mold shrinkage compared with many resins. A typical range for unfilled grades is roughly 1.8 to 2.2 percent, and it can run higher in thick sections. The final value depends on wall thickness, packing, mold temperature and gate size. Because of this, shrinkage factor is one of the first items to confirm at mold design review. See mold design review checklist.

POM also keeps shrinking for some time after molding as crystallization finishes. Plants usually allow a stabilization period, often 24 hours or more, before measuring critical dimensions. Agree on this in the sample plan. Parts that will be machined or assembled to tight fits need a stable measurement condition. See injection molding tolerances for tolerance classes and how to write them.

Design rules for POM parts

  • Keep walls even. Thick spots shrink more, void in the middle and sink. Aim for uniform walls, and core out thick bosses. Ribs at about half to two thirds of the adjoining wall limit sink. See injection molding wall thickness.
  • Add radii. Because POM is notch sensitive, round inside corners. A radius of at least a quarter to half of the wall is a common starting point.
  • Give draft. POM grips cores as it shrinks. One degree is common, and more helps on deep ribs and textured faces. See draft angle in injection molding.
  • Avoid sharp transitions between thick and thin sections.
  • Allow for snap fits carefully. POM’s stiffness and good fatigue life suit snap features, but the strain limit is modest. See snap fit design.

Gears and bearings: extra points

Gears are a leading use of POM, and they need more care than a plain housing.

  • Gate location. Gate in the center or use a diaphragm or several symmetric gates so shrinkage is even around the gear. One side gate makes the gear slightly out of round.
  • Weld lines. Avoid weld lines in the teeth. They weaken the gear root.
  • Tooth accuracy. Gears are specified by a gear quality grade from a standard. The mold must be cut with shrinkage compensation matched to the actual resin and the tooth geometry, and corrections often come after T1 sampling.
  • Material choice. A lubricated grade reduces friction and noise. For heavy loads or heat, consider whether nylon or a reinforced grade is better. See PA6 vs PA66.
  • Bearings and bushings. Specify the bore tolerance, surface finish and running clearance. Plastic bearings need a clearance that allows for expansion and for the shaft material.

Need a quote for a molded part? Get matched with a molding plant

Processing basics

The plant sets conditions from the resin supplier’s data. Typical ranges, which vary by grade:

  • Melt temperature: roughly 190 to 230 degrees C. POM decomposes if held too hot or too long.
  • Mold temperature: roughly 60 to 100 degrees C. Higher temperature gives better crystallinity, lower shrinkage variation and a smoother surface, but longer cooling.
  • Drying: POM absorbs little moisture. Many suppliers still advise drying or at least keeping the resin sealed, because surface moisture can cause splay.
  • Residence time: keep it short. Match the shot size to the barrel so material does not sit long.
  • Pressure and holding: enough to pack the part and reduce voids, with a gate that does not freeze too early.

Never mix POM with PVC

PVC and POM together in a barrel is a known hazard. PVC releases acidic gas on heating, which breaks down POM and releases formaldehyde. Plants should purge the machine fully before and after POM, use a compatible purge material and keep POM away from PVC scrap and regrind bins. Ask the plant to confirm its purge practice if the same press has run PVC. Good ventilation is part of safe POM processing.

Joining and finishing POM

POM’s low surface energy and chemical resistance make some finishing steps harder than with ABS or PC.

  • Ultrasonic welding works well on POM, because the material is rigid and melts sharply. Joint design and energy director shape matter.
  • Heat staking and press fits are common for posts and bushings. Press fits must allow for stress relaxation over time.
  • Adhesives need surface treatment and testing. Plan on mechanical joining instead.
  • Printing and painting need surface treatment or special inks. Laser marking works on some grades, and the color of the mark depends on the pigment.
  • Machining after molding is possible for tight bores, with the cost and time that adds. See injection molding secondary operations.

When POM is the wrong choice

Choose another resin if the part will:

  • Sit outdoors without UV protection.
  • Contact strong acids, strong bases or oxidizing agents, including chlorinated water at higher concentrations. A copolymer grade rated for the exposure is the first thing to check.
  • Need flame resistance. POM burns, and flame retardant POM is not a standard route.
  • Run near its upper temperature limit under load for long periods.
  • Need glue-bonded joints with high strength.

In those cases a nylon, PBT or a high temperature resin may serve better, and the plant can advise on cost and processing.

Quality checks

For gear and bearing parts, ask for:

  • Dimensional report on critical bores, gear form and runout, with measurement method and conditions.
  • Material certificate and lot number.
  • Weight check as a quick process indicator.
  • Visual check for voids, sink and flow marks. Section a few parts to look for central voids.
  • A functional test on a mating part or gauge.

The same sample plan applies as for other molds: see T1, T2 and T3 mold trials and first article inspection for plastic parts.

What to put in the RFQ

  • Full POM grade name and color, homopolymer or copolymer.
  • Application: load, speed, lubrication, temperature, chemical exposure.
  • Critical dimensions with tolerances, and measurement condition.
  • Gear data: module, tooth count, quality grade, if applicable.
  • Wear or noise targets, and how you test them.
  • Annual volume and order quantity per release.

Send the part for quoting

plasticmoldingfactories.com is a manufacturers’ representative for audited plastic injection molding plants. Buyers pay nothing; the plant pays us a commission on orders from buyers we introduce. Send the drawing, grade and volume as an RFQ and we route it to the one partner plant whose lane fits, and you place the order with that plant directly.

Frequently asked questions

Can POM be glued?

Poorly. POM has a low surface energy and chemical resistance that make adhesives hard to use without surface treatment. Mechanical fastening, snap fits, ultrasonic welding, heat staking and insert molding are more common ways to join POM parts.

Is POM suitable for outdoor use?

Only with a UV stabilized grade, and even then with limits. Standard POM degrades under sunlight, with surface chalking and loss of toughness. If the part sits outdoors, ask for a grade stated for UV exposure and review its test data.

Why do POM gears need a specific gate location?

Shrinkage differs along and across the flow direction. A gate on one side makes the gear slightly out of round, which affects tooth accuracy and noise. Plants use a center gate, a diaphragm gate or several symmetric gates to keep the shrinkage even.

Need a quote for a molded part?

Send the model. We match it to the partner plant whose lane fits and reply within 24 business hours. Free for buyers.

Get matched with a molding plant

Keep reading