Guides / Materials
PA6 vs PA66 glass filled: strength, heat, moisture and which to specify
November 9, 2026
PA6 (nylon 6) and PA66 (nylon 66) are both polyamides with glass fiber options, and both are used for brackets, housings, gears, clips and automotive parts. The short answer: choose PA66 glass filled when you need higher stiffness and better heat resistance, and choose PA6 glass filled when impact toughness, surface appearance or processing latitude matter more. Both absorb moisture, and that affects dimensions and properties more than the choice between them.
Figures here are typical for general grades. Datasheets for specific grades differ, and values depend on the test method and moisture condition.
PA6 vs PA66 at a glance
| Property | PA6 | PA66 |
|---|---|---|
| Melting point | About 220 degrees C | About 260 degrees C |
| Heat deflection with 30 percent glass (typical) | Lower, roughly 200 degrees C range | Higher, roughly 250 degrees C range |
| Stiffness and strength | Good | Slightly higher |
| Impact toughness | Better | Slightly lower |
| Moisture uptake at equilibrium in air | About 2.5 to 3 percent unfilled | About 2.5 percent unfilled |
| Moisture uptake when saturated in water | About 9 to 10 percent unfilled | About 8 to 9 percent unfilled |
| Mold shrinkage | Slightly lower | Slightly higher |
| Surface with glass | Generally better | Generally rougher |
| Cycle time | Slower to crystallize | Faster, can cut cycle time |
| Processing temperature | Lower barrel temperatures | Higher barrel temperatures |
| Resin cost | Usually lower | Usually higher |
Moisture figures are for unfilled grades. With 30 percent glass, the nylon content is lower, so uptake drops roughly in proportion. Cost depends on market conditions, so compare quotes for the exact grades.
Strength, stiffness and heat
PA66 has a higher melting point and a more tightly packed crystal structure, which gives it higher stiffness and higher heat deflection temperature. With 30 percent glass, PA66 is commonly chosen for parts that see continuous high temperature, such as under-hood components, power tool housings and electrical parts that heat up.
PA6 glass filled is still strong and stiff, and it is often tougher. It tolerates shock and repeated flexing better. For snap fits and clips, PA6 can be the safer choice because it is less brittle when dry.
If heat resistance is the main requirement, test the real part at temperature. A heat deflection temperature number is a screening figure, not a design limit. Ask for creep data at your temperature and load.
Moisture: the property that surprises buyers
Nylon is hygroscopic. It absorbs water from the air, and the water acts as a plasticizer: stiffness and strength drop and toughness rises. Parts also swell by a small amount as they absorb.
Two states matter.
- Dry as molded (DAM): right after molding, parts are dry. They are stiff and slightly brittle. Datasheets list these values first.
- Conditioned: after parts reach moisture equilibrium with room air, often over days to weeks depending on thickness. Properties settle at lower stiffness and higher impact.
Both PA6 and PA66 follow this pattern. PA66 takes up slightly less water, but the difference is small compared with the effect of the design environment. For parts used in humid conditions or in contact with water, design on the conditioned values, not the DAM figures.
Dimensional change can matter in tight fits. Unfilled nylon can grow on the order of a few tenths of a percent as it reaches equilibrium. Glass filled grades grow less, and the change is uneven because fibers restrain swelling along the flow direction. Agree with the plant whether dimensions apply as-molded or conditioned, and how parts are conditioned before measurement. See injection molding tolerances for how to set tolerances on shrinking resins.
Shrinkage and warpage
Both resins are semi-crystalline, so shrinkage is higher than for amorphous plastics, and glass fibers add a directional effect: parts shrink less along the flow direction (the way fibers align) and more across it. That mismatch pulls flat parts out of shape.
PA66 crystallizes quickly and often shrinks a bit more. PA6 crystallizes more slowly, which gives a wider processing window but can mean longer cooling. For flat parts, ask the plant how it will handle gate location, rib layout and mold temperature to control warpage. Read warpage in injection molding for the main causes.
Processing differences
- Drying. Both must be dried before molding because moisture causes splay, voids and loss of molecular weight. Typical practice is a desiccant dryer at about 80 degrees C for several hours to reach a very low moisture level. Always follow the supplier’s data sheet. See the resin drying temperature chart.
- Barrel temperature. PA66 runs hotter than PA6 because of the higher melting point. Excess heat or long residence time degrades both.
- Mold temperature. Glass filled nylon typically runs a warm mold, often in the range of about 80 to 120 degrees C. A warm mold gives better surface finish and more even crystallinity.
- Wear. Glass fiber is abrasive and wears screw, barrel, gates and mold steel. Plan hardened wear parts. See glass filled nylon injection molding and P20 vs H13 mold steel.
Need a quote for a molded part? Get matched with a molding plant
Surface appearance
Glass fibers can float to the surface and give a rough, fibrous look called glass bloom. PA6 grades generally give a better surface than PA66 at the same glass level, and a hot mold helps both. If the surface is visible, specify the finish and ask for samples. A texture can hide fibers.
Cost and supply
PA66 usually costs more than PA6 and its price can change with supply of its raw materials. This makes PA6 attractive where the extra performance of PA66 is not needed. For a real comparison, ask the plant to quote both grades. Include the cycle time, since faster crystallization of PA66 can offset part of the resin cost.
Beyond price, check which grades the plant can source reliably. Some applications also require specific approvals such as UL flammability ratings, which are listed by the exact grade and color, see UL 94 V-0 plastic.
Testing and approvals
Do not choose on datasheet numbers alone. Ask the plant to mold test bars or the real part and test them in the condition of use. For brackets and housings, a simple load test at the working temperature, on conditioned parts, tells more than a table. If the part has a flammability, food or electrical approval, confirm that the approval covers the exact grade, color and thickness, and that the plant uses that grade. A color change can void a listing.
Also agree what the plant does if the supplier changes the grade or discontinues it. Nylon grades are updated from time to time, and a replacement may behave differently in shrinkage and surface.
When to choose which
Choose PA66 glass filled when:
- Continuous temperature is high and stiffness at heat matters.
- The part carries load under heat, for example a bracket near an engine or heater.
- Fast cycle time is important.
Choose PA6 glass filled when:
- Impact, snap fits or repeated flexing matter more than the last bit of stiffness.
- A better surface is needed.
- A wider processing window and lower cost matter.
Consider other resins when: moisture sensitivity is a problem. PBT, PPA or POM may hold dimensions better in humid conditions. See POM acetal injection molding for one alternative.
What to put on the drawing and PO
- Resin: PA6 or PA66, glass percent by weight and the supplier grade or an approved equivalent list.
- Color: natural, black or a masterbatch, and whether it must match.
- Moisture condition for dimensions and tests.
- Regrind limit, if any.
- Test requirements: tensile, impact or flammability, with the standard and the conditioning.
- Surface finish on visible faces.
If you do not name the grade, the plant chooses one and your property data may differ from your assumptions. For more on how to write the package, see what to send for an injection molding RFQ.
Next step
We are a manufacturers’ representative for audited plastic injection molding plants. Buyers pay nothing: the plant pays us a commission on orders from buyers we introduce. Send an RFQ with the resin, glass content and operating conditions, and we match it to the one partner plant whose lane fits.
Frequently asked questions
Is PA66 always stronger than PA6?
At equal glass content, PA66 is usually stiffer and holds its strength to a higher temperature. PA6 is often tougher and handles impact better. Strength figures from datasheets also depend on moisture, so compare dry-as-molded and conditioned values for both.
How much glass should I specify?
Glass filled nylon commonly comes with 15, 30 or 50 percent glass by weight, with 30 percent the most common. More glass adds stiffness and strength but lowers impact, increases anisotropic shrinkage and wears the mold faster. Choose the lowest level that meets the load case.
Why did my nylon parts change size after shipping?
Nylon absorbs moisture from the air and grows slightly as it does. Parts measured right after molding are dry and slightly smaller than parts conditioned at room humidity. Agree whether the drawing dimensions apply dry or conditioned, and how the plant should measure.
Need a quote for a molded part?
Send the model. We match it to the partner plant whose lane fits and reply within 24 business hours. Free for buyers.
Get matched with a molding plant