Skip to content
Get matched

Guides / Materials

Resin drying temperature chart: typical times, temperatures and moisture limits by material

November 21, 2026

The right drying settings depend on the exact grade, so the resin supplier’s datasheet is the final authority. As a typical starting point, ABS dries at about 80 to 85 degrees C for 2 to 4 hours, PC at about 120 degrees C for 3 to 4 hours, PA6 and PA66 at about 80 degrees C for 4 to 6 hours and PET at about 120 to 160 degrees C for 4 to 6 hours. The chart below lists these and more, with the moisture level each material needs before it goes into the barrel.

Why drying matters

Many engineering resins absorb water from the air. Hygroscopic resins such as nylon, PC and PET take up moisture in the warehouse, in an open bag, or even in a hopper without a lid. When wet pellets are heated in the barrel, two things happen.

  • Steam. Water turns to vapor and shows on the part as splay, silver streaks or bubbles (see splay in injection molding).
  • Hydrolysis. In PC, PET, PBT and nylon, water at melt temperature breaks polymer chains. The part looks fine and then fails. Impact strength, elongation and fatigue life drop, and no visual check will find it.

The second problem is the more serious one for buyers. A cosmetic defect is caught at the end of the line. A part made from wet PC or wet PET can pass dimensions and still crack in the field.

Typical drying chart

Values are typical starting points, not specifications. Grades with glass fiber, flame retardants or special additives can differ. Always check the datasheet for the grade on your purchase order.

Resin Typical drying temp (C) Typical time (hours) Typical moisture target before molding Notes
ABS 80 to 85 2 to 4 Below about 0.1% Splay is the usual sign of wet ABS
PC About 120 3 to 4 Below about 0.02% Hydrolysis lowers impact strength
PC/ABS 90 to 110 3 to 4 Below about 0.04% Follow the grade sheet, blends differ
PA6 About 80 4 to 6 Below about 0.2% Vacuum or dry air; too much heat in air yellows it
PA66 About 80 4 to 6 Below about 0.2% Glass filled grades dry the same way
PET 120 to 160 4 to 6 Around 0.005% (50 ppm) or lower Very sensitive; crystalline pellets need higher temperature
PBT About 120 2 to 4 Below about 0.04% Hydrolysis risk like PET
PMMA About 80 3 to 4 Below about 0.1% Bubbles and haze if wet
POM (acetal) 80 to 100 2 to 3 Often only needed if stored damp Low moisture uptake
TPU 80 to 110 2 to 4 Below about 0.02% Wet TPU gives bubbles and weak parts
PEI, PSU, PEEK 120 to 160 3 to 4 Datasheet value High temperature dryer needed
PP, PE, PS Usually none None Low by nature Dry only if surface moisture is present

Reading the table: the temperature and time must be used together with the right air. Time at temperature starts when the pellets reach that temperature, not when the dryer is switched on. A hopper that holds resin for less than the drying time gives wet resin to the press at the bottom, however hot the air is.

Dryer type matters

Three dryer types are common in molding plants.

  • Hot air oven or hopper dryer. Heats ambient air. Works only for resins that need no deep drying and in dry climates. It cannot dry nylon or PET to target on a humid day.
  • Desiccant (dehumidifying) dryer. Passes dried air, usually at minus 30 to minus 40 degrees C dew point, through the hopper. This is the standard for hygroscopic resins.
  • Vacuum dryer. Dries at lower temperature under reduced pressure. Useful for heat-sensitive resins and fast changeover.

In a hot, humid climate like southern Vietnam, a plant that molds nylon, PC or PET without desiccant drying is taking a real risk. The ask is simple: which dryer feeds which press, what dew point does it log, and when was the desiccant bed last regenerated or replaced.

Sizing: hopper volume and throughput

The hopper must hold enough resin for the full drying time at the actual consumption rate. A simple check:

  1. Find the shot weight and cycle time, and compute resin used per hour.
  2. Multiply by the drying time in hours.
  3. Compare to the hopper capacity. If the hopper is smaller, the resin leaves early.

For example, a press using 6 kg per hour with a 4 hour drying time needs a hopper that holds at least 24 kg of resin. A small molding machine dryer is not a fix for a large job. A plant that quotes a shorter cycle than the dryer can support is a warning sign.

Need a quote for a molded part? Get matched with a molding plant

How to confirm that the resin is dry

Time and temperature are inputs. Moisture is the result. Three practical ways to check:

  1. Loss-on-drying moisture analyzer. A small instrument that heats a pellet sample and measures weight loss. Fast and common in plants that mold PC, PET and nylon.
  2. Karl Fischer titration. More accurate, mostly used in a lab or for very low targets such as PET.
  3. Dew point log. Not a direct reading of the resin, but a trend that shows the dryer is working.

Start-up checks matter most. After a long shutdown, a color change or a bag change, take a sample from the hopper outlet and record the result before running production.

Handling after drying

Dried resin picks up moisture again. PA can pick up a noticeable amount within minutes in humid air, and PET and PC in not much more time. Keep dried material in a closed hopper with a dry air loader, and avoid carrying it in open buckets. Bags opened and not used must be resealed.

Regrind needs drying too. Regrind has a high surface area and has been exposed to air, so it often absorbs more moisture than fresh pellets. The regrind ratio and drying of regrind should be written in the process sheet. Masterbatch and additives carry moisture and can be dried with the base resin where the datasheet allows.

Over-drying also does harm. Nylon dried too hot in air can yellow, and some resins stick in the hopper if the temperature is above the datasheet. For recycled grades, see PCR plastic injection molding for how lot variation changes the picture.

Wet resin symptoms and what they point to

Symptom Likely cause linked to moisture First check
Silver streaks, splay Water vapor in melt Resin moisture reading, hopper time
Bubbles or voids in thick parts Moisture or trapped gas Moisture, then venting and back pressure
Brittle parts, cracked on drop test Hydrolysis in PC, PET, PBT or PA Moisture history, melt viscosity or intrinsic viscosity test
Flash, very low melt viscosity Chain breakdown from wet resin Moisture, then clamp and pack
Shot weight drifts Variable moisture in feed Dryer log, regrind ratio

For PC parts specifically, read polycarbonate injection molding for wall thickness, stress and drying together. For nylon, PA6 vs PA66 covers how each grade absorbs water and how that moves dimensions in service.

What to ask the plant

  • Which resin grade and drying setting do you use for our part, and where is it written?
  • What dryer type feeds the press, and what dew point does it log?
  • How do you check moisture at start-up and after a long stop?
  • How do you handle regrind and masterbatch?
  • Can you share drying and process records for the T1 trial?

You are not looking for perfect answers. You are looking for a plant that has the numbers and keeps records. A plant that answers “we dry as the datasheet says” with a number and a log is better than one that says “we always dry it.”

Next step

Put the resin grade, drying requirement and moisture check in your RFQ and quality agreement so the plant prices it. If you want a plant whose lane fits an engineering resin job, send an RFQ. We are a manufacturers’ representative for audited plastic injection molding plants: we route your request to the partner plant whose lane fits, buyers pay nothing, and the plant pays us a commission on orders from buyers we introduce.

Frequently asked questions

Can I dry resin longer than the datasheet says?

Usually a small overrun is harmless, but long exposure at high temperature can discolor nylon, degrade some additives and make pellets stick together. Follow the resin supplier's datasheet for temperature and time, and use a moisture reading rather than extra hours to confirm the resin is ready.

Does polypropylene need drying?

PP, PE and PS absorb very little moisture, so they normally do not need drying. They can still carry surface moisture if bags were stored cold and opened in a warm humid room. Fillers, colorants and some regrind change the picture, so follow the datasheet for the exact grade.

What is dew point and why does it matter?

Dew point is the moisture level of the drying air. A desiccant dryer typically delivers air around minus 30 to minus 40 degrees C dew point. Hot air with a poor dew point cannot pull moisture out of pellets, so a hot hopper alone is not drying.

Need a quote for a molded part?

Send the model. We match it to the partner plant whose lane fits and reply within 24 business hours. Free for buyers.

Get matched with a molding plant