Skip to content
Get matched

Guides / Tooling

P20 vs H13 vs S136 mold steel: hardness, life, polish and cost compared

November 12, 2026

P20 is a pre-hardened tool steel for molds with moderate volume. H13 is a harder steel, heat treated, for long runs and abrasive resins. S136 is a stainless mold steel, hardened, for mirror polish, clear parts and corrosive resins. In short: use P20 when volume is moderate and the resin is unfilled, H13 when the program is long or the resin has glass fiber, and S136 when polish or corrosion decides. The sections below give typical numbers and the trade-offs.

All numbers here are typical and vary with the exact grade, the steel supplier and the heat treatment. Treat them as a way to compare, and ask the plant for the specification it will use.

Comparison table

P20 (and similar, such as 718H) H13 S136 (stainless, AISI 420 type)
Delivered state Pre-hardened Annealed, then heat treated Annealed, then heat treated
Typical working hardness About 28 to 36 HRC About 44 to 52 HRC About 48 to 54 HRC
Wear resistance Moderate High High
Polishability Good Good to very good Excellent, mirror finish
Corrosion resistance Low Low to moderate High
Typical mold life Up to a few hundred thousand shots Up to a million shots or more Up to a million shots or more
Cost of steel and machining Lowest Higher Highest
Ease of modification Easy, weldable Harder, needs care Harder, needs care
Main use General molds, moderate volume Long runs, glass filled resins Clear parts, medical, PVC and corrosive resins

Mold life is a typical planning range, not a promise. It depends on the resin, the maintenance and the mold design.

P20: the general purpose choice

P20 arrives from the mill at working hardness, so the tool shop can machine it without heat treatment. There is no distortion from quenching, delivery is quick and modifications are straightforward. If the part design changes after T1, welding and re-cutting P20 is routine.

Good fit:

  • Unfilled commodity and engineering resins such as PP, ABS, HDPE and PC, where wear is slow.
  • Moderate annual volumes, where the mold will not run millions of shots.
  • Prototypes that may become production tools.
  • Large molds where heat treating would be expensive or risky.

Limits: soft for glass filled resins, which wear gates and shut-off surfaces; can rust if not protected; the polish is good but not at optical level. Where you need a texture, P20 takes it well, see injection mold texture.

Variants such as 718H have higher nickel content and give a more uniform hardness through thick blocks, which is useful for large molds.

H13: for wear and long programs

H13 is a hot work tool steel used widely for mold cavities, cores and inserts that face heavy wear. It is machined roughly, heat treated to hardness, then finished by grinding, EDM and polishing. Because it is hard, it resists the abrasive action of glass fiber and mineral filled resins.

Good fit:

  • Glass or mineral filled resins such as GF nylon, GF PBT and GF PP, which erode soft steel at gates and parting lines.
  • Long production programs with high annual volume.
  • Inserts and slides that see repeated sliding wear.
  • Molds with thin steel sections that need strength.

Limits: higher cost; heat treatment adds a step and a few days to weeks; there is a risk of distortion and cracks if heat treatment is poor; modifications are harder because the steel is hard. Ask whether the plant heat treats in house or uses a specialist, and whether the steel is vacuum hardened for stable results.

A common compromise is a P20 mold base and cavity with H13 inserts at the wear points such as gate areas and shutoffs. This keeps the cost closer to P20 while protecting the parts that wear first.

S136: for polish and corrosion

S136 is a stainless steel with high chromium content. When hardened, it takes a very high polish and keeps it, because it resists the rust and pitting that dull other steels. It is the usual choice for optical parts, clear housings, lenses and cosmetic parts with a mirror finish. For the polish grades used on drawings, see SPI surface finish.

It also suits resins that release corrosive gases when melted, such as PVC, and molding in humid conditions or with water cooling that causes rust.

Limits: highest cost; more difficult to machine and weld; it needs careful heat treatment and polishing by skilled people. Do not specify S136 for a part that does not need the polish or corrosion resistance. It is not required for a textured, hidden or low cosmetic part.

Other steels you may hear

  • NAK80 and similar precipitation hardened steels: pre-hardened to around 40 HRC, take a good polish and need no quenching. Common for cosmetic parts and fine textures.
  • Beryllium copper and aluminum alloys: used as inserts for cooling hot spots, or as prototype mold material. See aluminum vs steel injection mold.
  • Hardened tool steels such as D2: used for cutting edges, slides or wear inserts.

These names are shortcuts. Ask for the exact grade and the certificate, since the same name can cover different composition and quality levels.

Need a quote for a molded part? Get matched with a molding plant

How the steel affects cost

The steel price is only part of the effect. Harder steels cost more to machine, wear cutters faster and require more EDM time. Heat treatment adds both time and cost. Polishing stainless takes longer. A mold in H13 or S136 can cost noticeably more than the same mold in P20. See injection mold tooling cost for how steel fits into the full price.

On the other side, hardened steel can lower cost over the life of the program if it avoids repairs and downtime, particularly for abrasive resins.

How to choose

Answer these in order:

  1. What is the resin? If it is glass filled, mineral filled or flame-retardant with abrasive fillers, start with H13 at least at wear points.
  2. What is the total shot count over the program? If it is below a few hundred thousand shots on unfilled resin, P20 is usually enough.
  3. How good must the surface be? For mirror finish or clear parts, consider S136 or a polish grade steel.
  4. Is corrosion a risk? PVC, humid storage or corrosive additives point to stainless.
  5. How likely is a design change? If the design may change, P20 is easier to modify.

If the plant proposes a steel, ask why. If the quote does not state steel, ask. Compare quotes only when the steel is the same, as covered in how to compare injection molding quotes.

A worked example

Take a housing in unfilled ABS, a 2-cavity mold and a plan for 150,000 parts over three years. The shot count is about 75,000 per cavity set, far below the typical life of P20. P20 is the sensible choice, and the money saved can go into a hot runner or better cooling.

Now take a connector body in 30 percent glass filled nylon, with 1 million parts a year for five years. The glass will erode gates and shut-offs within a short time in soft steel. Here H13 for the cavity, core and gate inserts is the safer choice, and the plant should state a maintenance interval for the gates. If the same program also needs a clear lens on the front, that single insert may be S136 while the rest stays in H13. Mixed steels in one mold are normal. Ask the plant for a steel map that lists each component and its grade.

What to put on the PO

  • Steel grade and hardness for cavity, core and slides.
  • Whether inserts at gates and shut-offs use a harder steel.
  • Expected mold life in shots, with the resin it assumes.
  • Steel certificates and heat treatment records.
  • Polish or texture per face.

Mold class under the SPI system also sets expectations for life and use, see SPI mold classification. Wikipedia’s article on tool steel is a neutral reference for grade names.

Send us the part

We are a manufacturers’ representative for audited plastic injection molding plants. Buyers pay nothing: the plant pays us a commission on orders from buyers we introduce. If you are not sure which steel your program needs, send an RFQ with the resin, annual volume and finish, and we match it to the one partner plant whose lane fits.

Frequently asked questions

How many shots can a P20 mold run?

A P20 mold on an unfilled resin often runs in the range of a few hundred thousand shots with normal maintenance. Glass filled resins wear it faster. Treat any shot count as a typical planning figure, and ask the plant to state the expected life for your resin and part.

Is H13 always better than P20?

No. H13 is harder and lasts longer, but it costs more to buy and to machine and often needs heat treatment, which adds time and risk of distortion. For moderate volumes on unfilled resin, P20 is usually enough and easier to correct.

Do I need S136 for clear parts?

For optical clarity or a mirror polish, a stainless steel such as S136 is the usual choice because it takes a high polish and resists staining and rust. Other polishable steels exist, so ask the plant what it proposes and what surface finish it can hold.

Need a quote for a molded part?

Send the model. We match it to the partner plant whose lane fits and reply within 24 business hours. Free for buyers.

Get matched with a molding plant

Keep reading