Skip to content
Get matched

Guides / Design

SPI surface finish grades explained: what A, B, C and D mean for your molded part

November 21, 2026

SPI surface finish is a grading system for the surface of an injection mold, from the highest mirror polish (A-1) to a coarse dry-blasted texture (D-3). The grade names the method used to finish the mold steel, and the plastic part copies that surface when it is molded. Specifying the grade on the drawing, per face, tells the toolmaker how much hand work to build in and tells the buyer what the part will look like. It also decides a large share of the finish cost of the mold.

What the SPI letters mean

The standard comes from the Society of the Plastics Industry, now the Plastics Industry Association. It sorts mold finishes into four groups by the tool used on the steel.

  • A grades: polished with diamond compound or paste. Mirror finish.
  • B grades: sanded with fine grit paper. Semi-gloss.
  • C grades: stoned with abrasive stones. Matte with visible fine lines.
  • D grades: dry blasted with glass bead or aluminum oxide. Satin to rough matte.

Each group has three numbers (1 to 3) from finest to coarsest.

SPI finish chart

The table shows the method and a typical roughness range. Roughness values are approximate and commonly cited, not guaranteed. They are measured on the mold steel and vary with the steel, the toolmaker and the measuring method.

Grade Method Typical Ra on mold (micrometers) Look and typical use
A-1 Grade #3 diamond buff about 0.01 to 0.02 Mirror. Lenses, optical parts, display covers
A-2 Grade #6 diamond buff about 0.02 to 0.04 High gloss. Clear covers, cosmetic gloss
A-3 Grade #15 diamond buff about 0.05 to 0.10 Gloss. Cosmetic housings, shiny trim
B-1 600 grit paper about 0.05 to 0.10 Semi-gloss. Visible parts, light polish look
B-2 400 grit paper about 0.10 to 0.15 Semi-gloss. General cosmetic parts
B-3 320 grit paper about 0.28 to 0.32 Satin. Moderate cosmetic need
C-1 600 grit stone about 0.35 to 0.40 Fine matte. Non-cosmetic with clean look
C-2 400 grit stone about 0.45 to 0.55 Matte. Internal or technical parts
C-3 320 grit stone about 0.63 to 0.70 Matte, visible tool lines. Hidden parts
D-1 Dry blast glass bead about 0.80 to 1.00 Satin matte. Hides small flaws
D-2 Dry blast fine oxide about 1.00 to 2.80 Dull matte. Hides flow lines and marks
D-3 Dry blast coarse oxide about 3.20 to 18.0 Rough matte. Grip surfaces, hides sink and weld lines

Treat the numbers as a reference point. The grade, not the Ra value, is what the drawing should call out. If the buyer needs a measured roughness, say so separately and agree where and how it is measured.

Choosing a grade by purpose

For optical or mirror parts

Only A-1 and A-2 give true optical clarity. These parts need a stainless or high-polish mold steel, a clean environment, an excellent mold and careful molding. Any flow mark, ejector mark, dust particle or parting line shows. Plan for higher mold cost, longer finishing time and a smaller process window. Clear resins such as PC and PMMA also need drying and clean handling.

For visible consumer or industrial housings

B grades or A-3 suit most cosmetic housings. They look polished without the cost and fragility of A-1. B-2 or B-3 hides minor tool lines. Gloss shows defects such as sink marks, weld lines and flow marks very clearly. If the part has ribs or bosses on the back, expect sink risk on a glossy front face. For causes and fixes, see sink marks in injection molding.

For hidden or technical parts

C grades are cheap and good enough for faces nobody sees. A machined finish with light stoning is often sufficient. Specify “as machined” or “light stone” for internal faces to avoid paying for polish.

For hiding defects and giving grip

D grades are blasted and hide small flaws, so they are common on handles, enclosures and tools. D-2 and D-3 also reduce visible flow lines and knit lines. They need more draft because the surface grips the part. For a more developed texture system (leather grain, geometric patterns) see injection mold texture.

How the finish shows up in the part

The part is a copy of the mold, but the copy is never perfect.

  • Resin: amorphous resins such as PC, ABS and PMMA reproduce polish well. Semi-crystalline resins such as PP and PA reproduce it less sharply. Glass fibers and mineral fillers roughen the surface and dull the gloss. Some colors, especially dark ones, show scratches and marks more.
  • Molding conditions: a hot mold and good packing give higher gloss. Cold molds and short fill leave dull areas, flow marks and halos.
  • Wear: a high polish wears. Over time, gloss falls and the surface may show scratches from cleaning or from glass filled resin. Ask the plant how polish will be protected between runs.
  • Direction: polishing and stoning leave directional marks. For some surfaces the direction of marks matters for demolding or appearance. Draw on the drawing the direction if it matters.

Need a quote for a molded part? Get matched with a molding plant

Steel and polish

A mirror finish needs a steel that polishes cleanly. Hardened and stainless mold steels (see P20 vs H13 mold steel) generally polish better than standard pre-hardened steel, especially premium grades that are cleaner and have fewer inclusions. Tell the plant if you need a high polish so they quote the right steel. A cheap mold with a mirror requirement often leads to “orange peel” or pitting on the polished face.

How to specify finish on a drawing

Put the SPI grade on the face or on a note, not just a general note. A drawing with “all surfaces SPI A-2” costs far more than one that polishes only the visible face.

A good note says:

  1. Face: which face or area (use a reference such as “visible face A, see model”).
  2. Grade: for example SPI B-2.
  3. Direction (if needed): polish direction.
  4. Exclusions: areas with no finish requirement, such as parting line, shut-off faces and gate area.
  5. Acceptance: how the buyer will judge the finish (a master sample, a photo or a gloss meter value).

Without an acceptance method, finish becomes an argument. A sample signed by both parties is the cleanest standard. Gloss meter readings help, but they also depend on resin and color.

Finish and cost

The more labor and time the surface takes, the more the mold costs.

  • A and B grades add polisher hours. A-1 can take days on a large face.
  • D grades are cheap and fast, since blasting is quick.
  • A high polish can be lost in a repair. A weld repair on a mirrored cavity needs re-polishing.
  • Textures need extra draft and sometimes bigger steel allowances. They are often done by specialist shops, which adds time.

See injection mold tooling cost for how finish sits next to cavities, steel and side actions in a full mold quote.

Design details that help the finish

  • Add draft. Polished faces need at least 0.5 to 1 degree. Blasted faces often need 1.5 to 3 degrees or more. See draft angle in injection molding.
  • Keep wall thickness even. Uneven walls cause sink and gloss changes.
  • Place gates and ejector pins away from the cosmetic face. Ask the plant where gate vestige and ejector marks will fall.
  • Avoid sharp internal corners on polished faces. They are hard to polish and they trap marks.
  • Plan parting lines. The parting line cannot be perfectly polished. Place it where it will not distract.

Where we fit

We are a manufacturers’ representative for audited injection molding plants. Buyers pay us nothing; the plant pays a commission on orders from buyers we introduce. If you have a part with a finish requirement, send an RFQ with the grade per face and we route it to the partner plant whose lane fits.

Frequently asked questions

Is SPI A-1 always the best finish to choose?

No. A-1 is the highest polish and the most expensive to make and keep. It shows every flaw in the part and the mold, so it needs the right steel, clean molding and careful handling. Use it only on faces that need optical clarity or a mirror look, and specify a lower grade elsewhere.

Can any resin take any SPI finish?

The mold surface can be made to any grade, but the part will look different by resin. Glass filled resins do not reproduce a high polish well because fibers and pigments break the surface. Soft resins such as TPE look duller than the mold. Ask for a sample before committing.

Do I need a different draft angle for rough SPI grades?

Yes. Matte blasted grades such as D-2 and D-3 grip the part during ejection and need more draft than a polished face. Confirm the draft with the plant at design review, and see the separate guidance on texture draft.

Need a quote for a molded part?

Send the model. We match it to the partner plant whose lane fits and reply within 24 business hours. Free for buyers.

Get matched with a molding plant

Keep reading