Guides / Design
Injection molding gate types and gate location: how to choose the gate and where to put it
November 6, 2026
The gate is the small opening where melt enters the cavity, and its type, size and location decide how the part fills, packs and cools. Pick the gate for the part: an edge gate is the default for flat or boxy parts, a submarine gate suits automatic degating, a pin point gate gives a small mark in the middle of a part, a fan gate spreads melt across a wide flat face and a valve gate gives the cleanest mark on cosmetic parts. Put it where the part is thickest, aim the flow at a wall and keep the mark off cosmetic faces.
This guide lists the common gate types, how big a gate should be and the rules for choosing location. It also shows what to put on the drawing and what to ask the plant.
What the gate does
The gate controls three things:
- Fill. Where the melt enters decides the flow pattern, the weld lines and the air traps.
- Pack. A gate that freezes too early stops packing and leaves sink marks or voids.
- Cosmetics. Every gate leaves a mark, called the vestige, that you may need to hide or trim.
Gate choice also decides whether the runner is separated automatically, whether you need to trim by hand and how much material is wasted. For the runner side see hot runner vs cold runner.
Common gate types
| Gate | Where it sits | Strengths | Limits |
|---|---|---|---|
| Sprue gate | Directly from the sprue into the part | Simple, good pack, single cavity round parts | Large mark, hand trim, only single cavity |
| Edge gate | On the parting line at the edge of the part | Most common, easy to build and modify | Mark on the edge, trim by hand or tool |
| Tab gate | Edge gate through a small tab that is removed | Moves shear away from the part, reduces stress | Extra trim step |
| Fan gate | A wide, shallow gate on the parting line | Even fill of wide flat parts, less warpage | Wider mark and more trim |
| Film (flash) gate | Very wide, thin gate along an edge | Flat parts, low stress | Large trim area |
| Submarine (tunnel) gate | Angled tunnel below the parting line into the part | Degates automatically on ejection | Not for brittle or glass filled resins, wears |
| Cashew (banana) gate | A curved submarine gate | Gates inside surfaces from the moving side | Complex to build |
| Pin point gate | Small gate in a three-plate mold, top of the part | Central gating, small mark, balanced fill | Needs three-plate or hot runner, more waste |
| Diaphragm gate | A disk across the whole opening of a round part | Even fill around, no weld line | Must trim the disk |
| Ring gate | A ring around a core pin | Even fill for tubes | Trim all around |
| Hot tip gate | Hot runner nozzle with a small tip | Small mark, no cold runner | Needs hot runner |
| Valve gate | Hot runner nozzle with a moving pin | Cleanest gate, controlled packing | Cost and maintenance |
Not every type works with every resin. Submarine gates shear the melt and snap off the gate on ejection, which is a problem with brittle or glass filled grades. Hot tip gates suit crystalline resins that freeze cleanly and not stringy ones.
For hot runner choices see valve gate vs open gate hot runners.
Gate size
Size depends on resin, wall and part weight. These are typical starting points for edge gates and the plant adjusts after a trial.
- Depth (thickness): about 50 to 75 percent of the wall at the gate. Small enough to freeze after pack, large enough to feed it.
- Width: about 1.5 to 3 times the depth for general-purpose resins, wider for fan gates.
- Land length: the short channel before the part, about 0.5 to 1.0 mm. Longer land loses pressure.
- Diameter for a pin point or sprue gate: a fraction of the wall, with a minimum set by shear limits of the resin.
Start small and open up. Steel can be removed but not easily added, so a mold maker builds the gate steel-safe, small at first, and enlarges it after T1. That is why gate size on the first trial often differs from the final size. See steel safe mold design and corrections after T1.
Shear is the limit on gate size for some resins. PVC, flame retardant grades and heat-sensitive resins degrade if forced through a very small gate at high speed. Large gates are used for these.
Need a quote for a molded part? Get matched with a molding plant
Gate location rules
Location matters more than type. Use these rules.
- Gate into the thickest section. Flow from thick to thin so the thick section can be packed. A gate in a thin wall freezes before the thick area is packed and causes sinks. See sink marks: causes and fixes.
- Aim the flow at a wall or a core pin. Melt shooting into an open area can jet, forming a snake-like flow pattern and flow marks. Aim the gate so that the melt hits a surface and spreads.
- Keep the gate off cosmetic faces. Place it on an edge, on the back or under a feature that hides the vestige.
- Balance the flow length. For symmetric parts, gate in the center. For long parts, gate at the middle of the long dimension, so all areas fill at about the same time.
- Put the weld lines where they do no harm. Holes and cores cause weld lines where the flow splits and rejoins. Location of the gate decides where they fall. Keep them away from stressed or cosmetic areas. See weld lines and knit lines.
- Fill to the vents. The end of fill should be near a vent and the parting line so air can escape.
- Mind fiber orientation. In glass filled resins, fibers align with flow. The gate decides the direction, which affects strength and warpage.
- Think about trim. A gate on a rib or a flat edge is easier to trim than one in a curved face.
- Leave space for an ejector. A gate vestige should not coincide with an ejector pin mark.
Multiple gates
Large parts, long flow paths and thin walls often need more than one gate. The benefits are shorter flow, lower pressure and better pack. The cost is weld lines where the flows meet, and more complexity in balancing.
- Place gates so the weld lines fall on non-critical areas.
- With hot runner valve gates, sequential opening (cascade) can move the weld line and cut visible marks on large panels.
- Check the balance of flow between gates in a fill study. See mold flow analysis.
Gates in multi-cavity molds
In a multi-cavity mold, each cavity needs the same gate and runner path so that all parts fill at the same time and with the same pack. Unbalanced runners cause weight and dimension differences between cavities. See multi-cavity balance and cavity-to-cavity variation.
What to put on the drawing and in the RFQ
Give the plant the information it cannot guess:
- Faces where a gate mark is not allowed, marked on the drawing.
- A maximum height for the gate vestige, such as 0.3 mm proud of the surface.
- The preferred gate type if you have one, such as automatic degating.
- Any area where strength matters and weld lines are not allowed.
- Whether hot runner is acceptable.
Ask the plant to show the proposed gate location in the DFM or mold design review, and to state the weld line locations and the end-of-fill positions. The checklist is in the mold design review checklist.
Questions for the plant
- Which gate type and size are proposed, and why?
- Where will the vestige be and how high?
- Where do the weld lines fall?
- Is the gate steel-safe for the first trial?
- How will the gate be removed: automatically, by tool or by hand?
- Can we see a fill study if the part is large or thin?
A plant that answers these before it cuts steel is a plant that has thought about your part. If you want one that fits your part and resin, send an RFQ. We are a manufacturers’ representative: we route it to the partner plant whose lane fits, buyers pay nothing and the plant pays us a commission on orders from buyers we introduce.
Frequently asked questions
Who decides the gate location, the buyer or the plant?
Both should agree, and it should be written down at the mold design review. The plant knows what fills well. The buyer knows which faces are cosmetic, where strength matters and where a gate mark cannot appear. Mark the no-gate zones on the drawing and let the plant propose the location within them.
Does gate size affect part strength?
Yes. A gate that is too small can shear the melt, degrade the resin and freeze early, which leaves weak, under-packed parts. A gate that is too large leaves a bigger mark, takes longer to trim and may allow over-packing near the gate. The plant sets it by resin, wall and part size, and adjusts after the first trial.
Can the gate be changed after the mold is built?
Often yes if it needs to be made larger, since steel can be removed. Moving a gate or making it smaller needs welding or a new insert, which costs more and may leave marks. Plan gate location carefully before steel is cut and leave the gate steel-safe for the first trial.
Need a quote for a molded part?
Send the model. We match it to the partner plant whose lane fits and reply within 24 business hours. Free for buyers.
Get matched with a molding plant