Skip to content
Get matched

Guides / Materials

Masterbatch vs precolored resin: how to choose the coloring method for a molded part

November 21, 2026

Masterbatch is a concentrated pigment pellet that the plant doses into natural resin at the press. Precolored resin is resin that has already been compounded with the pigment, so the plant simply dries it and molds it. Masterbatch wins when you need several colors in small quantities or need to change color often. Precolored resin wins when one color runs in large volume and the shade must stay the same from lot to lot. Both can hit the same color. The difference is cost, flexibility and how much of the consistency you leave to the press operator.

How each method works

Masterbatch. A pigment concentrate is made by dispersing colorants in a carrier resin. The plant mixes it with natural resin at the machine throat, either by blending pellets in a hopper or by feeding it through a dosing unit. The share of masterbatch in the final mix is called the let-down ratio. Typical let-down ratios run from about 1 to 4 percent, and the supplier states the right figure for each color.

Precolored (compounded) resin. The resin maker or a compounder melts the base resin, adds pigment and additives in a twin-screw extruder, and pellets the result. The color is already mixed through every pellet. The plant has nothing to dose.

Liquid color is a third route. It is a pumped liquid pigment dosed at the throat. It suits large volumes of a single color in some polyolefin and styrenic parts, but it needs good dosing equipment and is less common in small plants. This article focuses on the two options most export molders actually offer.

Side by side

Factor Masterbatch Precolored resin
Color consistency Depends on dosing accuracy and mixing at the press Set at the compounder, usually the more uniform option
Minimum order Small, often a few kg to a few tens of kg per color Often a full lot, commonly hundreds of kg to a tonne or more (typical)
Lead time for a new color Short once the match is approved Longer, because the lot is compounded to order
Cost per kg of colored part Resin price plus let-down share of masterbatch price Usually a premium per kg over natural resin, but no dosing equipment or labor
Inventory One natural resin plus small bags of color One bag type per color, and a stock risk if volume drops
Many colors, low volume each Strong fit Weak fit, because of minimum lots
One color, high volume Fine if dosing is controlled Strong fit
Risk of streaks or shade drift Higher if dosing drifts or mixing is poor Lower

The cost row deserves a caution. Masterbatch looks cheaper per kg because the pigment is diluted. Once you add the dosing equipment, the labor of weighing and blending and the cost of scrap when the shade drifts, the gap often shrinks. For a high-volume single color it can reverse. For a low-volume color it rarely does.

Where color problems come from

Most color complaints trace back to one of four sources.

  1. Dosing error. If the let-down ratio drifts from 2 percent to 1.6 percent, the shade changes. A volumetric doser can drift as the pellet bulk density changes. A gravimetric doser that weighs each batch holds the ratio tighter.
  2. Poor dispersion. A masterbatch is mixed by the screw inside the press, which has less mixing power than a compounding extruder. Weak dispersion shows as streaks, specks or a cloudy look, most visible in dark and very light colors.
  3. Process changes. Higher melt temperature, longer residence time or a hotter hot runner can darken or shift some pigments. Organic pigments are less heat stable than inorganic ones. Resins that mold at high temperature, such as PC, PA and PEEK, need pigments rated for that heat.
  4. Base resin variation. The natural resin itself varies slightly from lot to lot. A pale natural lot gives a slightly different result than a yellowish one with the same masterbatch dose.

Glass fiber, mineral fillers and flame retardants also change how a color reads. A match approved in unfilled ABS will not carry over to glass-filled PA. Approve the match in the actual resin grade.

How to specify color

Words like “light grey” or a printed swatch do not make a standard. Give the plant something it can measure.

  • A physical standard. A color chip or a molded plaque in the correct resin, texture and gloss, signed by both sides. Molded plaques are better than paper chips because gloss and texture change how color looks.
  • A named reference. A Pantone or RAL number is a starting point only. It does not define a molded color, because the same code looks different on paint, paper and plastic.
  • Measured values. CIELAB values (L*, a*, b*) of the approved standard, with an allowed Delta E. Measurement is done with a spectrophotometer. State the illuminant (D65 is common), the observer angle and whether gloss is included.
  • A visual check condition. If people judge the part by eye, state the light booth and the viewing distance.
  • Metamerism. Two colors can match under one light and differ under another. If the part sits next to other parts or is seen outdoors, check under at least two light sources.

For a deeper look at agreed cosmetic limits, see golden samples and limit samples for cosmetic defects.

Need a quote for a molded part? Get matched with a molding plant

When to choose which

Choose masterbatch when:

  • You order several colors of the same part in modest quantities.
  • Color changes between runs are frequent.
  • Volume per color is too small to meet a compounder’s minimum lot.
  • The color is not tightly critical and a small shade range is acceptable.
  • The plant has gravimetric dosing and a record of controlling it.

Choose precolored resin when:

  • One color runs in large volumes for years.
  • The part is cosmetic and visible, and shade drift would cause rejects.
  • White, black or other unforgiving colors are used. Dark gloss black and bright white show every streak.
  • The part is regulated, and you want the colorant formulation controlled and documented at the compounder.
  • Several plants will mold the same part, and you want the same color regardless of site.

If you are unsure, start with masterbatch for the prototype and first production lots, then move to precolored once volume and color are proven. Treat the change as a material change. See injection molding tolerances for how shrinkage and dimensions can move with it.

Regulatory and performance checks

Colorants are additives, and additives carry rules.

  • Flame rating. A UL listing is tied to specific resin grades, thicknesses and often colors. A change of color or colorant package can fall outside the listing. See UL94 V-0 resins for electrical enclosures.
  • Food contact and toys. Colorants must comply with the relevant rules for the end market. Ask for a declaration that names the colorant and the market.
  • Heavy metals and restricted substances. Pigments based on lead, cadmium or hexavalent chromium are restricted in many markets. Request a restricted-substance declaration from the masterbatch or compound supplier.
  • UV and weathering. Some pigments fade outdoors, and some protect the resin from UV. For outdoor parts, specify the exposure and ask for the supplier’s weathering data.
  • Mechanical effects. Pigments can slightly affect impact strength, shrinkage and weld line strength. This is normally small, but it should be confirmed on parts, not assumed.

Drying and handling

Masterbatch with a different carrier resin than the base can change drying needs. If the base resin is hygroscopic, such as PC or PA, the colorant must be dried with it or it can bring moisture into the melt and cause splay. A universal carrier may not be right for every resin. Ask the plant which carrier is used and whether it suits your resin. Drying settings by resin are covered in resin drying temperatures and moisture limits.

Regrind adds one more variable. If the plant adds regrind to the part, the colorant dose must be adjusted because the regrind already holds pigment. Many cosmetic parts allow no regrind. State your limit in the PO.

What to put in the RFQ and PO

  • Resin grade and manufacturer, with natural or colored resin stated.
  • Color standard: the signed plaque and the measured Lab* with Delta E limit.
  • Coloring method (or “plant to propose”), plus a request for the let-down ratio and carrier if masterbatch is used.
  • Regrind limit.
  • Any flame, food, toy or restricted-substance requirement for the colored grade.
  • A rule that any change of colorant supplier, ratio or method needs written approval.

When you compare plants, ask each to state its coloring method and its dosing equipment on the quote. That keeps line items comparable. For more on side-by-side checks, see how to compare injection molding quotes line by line.

Next step

If you have a part with a color requirement and need a plant that can hold it, send an RFQ. We are a manufacturers’ representative: we match your request to the one partner plant whose lane fits, buyers pay nothing, and the plant pays us a commission on orders we introduce. You order from the plant directly.

Frequently asked questions

What Delta E should I ask for on a molded part?

It depends on the color and the part. Many buyers accept a Delta E of about 1.0 to 1.5 against the approved standard for general cosmetic parts and ask for tighter control on white, black or large visible faces. State the number, the illuminant and the measurement geometry on the drawing, because Delta E without those details cannot be checked.

Can I switch from masterbatch to precolored resin after the mold is approved?

Yes, but treat it as a process and material change. The color, gloss, flow and shrinkage can shift a little, so the plant should run a trial, compare against the approved color standard and get your written approval before changing production.

Does a colorant change the flame rating or food contact status of a resin?

It can. A flame rating listing may apply only to named colors, and food contact compliance depends on every colorant in the formulation. Ask for the listing or declaration that covers your exact color, not just the natural resin.

Need a quote for a molded part?

Send the model. We match it to the partner plant whose lane fits and reply within 24 business hours. Free for buyers.